ABWS-8 -45°|ABWS-8 60°|ABWS-8 -70° AWS楔块与探头
公司名称:深圳华清仪器仪表有限公司
公司电话:、
公司传真:0755-
专线电话:
Q Q :
公司地址:深圳市龙华新区三联路清泉二期15A2
公司网址:http://www.huaqing17.cn
图片89.png
AWS探头和楔块
AWS探头和楔块符合美国焊接协会的结构焊接规范对用于焊缝检测中的角度声束组合件提出的特殊要求。
Advantages
· Transducers and wedges meet or exceed the specifications as set forth by the AWS Code Section D1.1
· Snail wedges use industry accepted hole spacing
· Captive screws included with the transducer
· Accupath style wedges marked with a five line graticule to assist in locating the beam exit point
优势
•Transducers and wedges meet or exceed the specifications as set forth by the AWS Code Section D1.1
•传感器和楔满足或超出规格由AWS D1.1规定的代码段
•Snail wedges use industry accepted hole spacing
•蜗牛楔子使用行业公认的孔间距
•Captive screws included with the transducer
•螺钉包括与传感器
•Accupath style wedges marked with a five line graticule to assist in locating the beam exit point
•accupath式楔标有一五线辅助光束出口点定位
探头与楔块
AWS传感器
晶片尺寸英寸 |
频率 |
探头型号规ACCUSCAN |
探头型号规格CENTRASCAN |
蜗牛形楔块型号
|
accupath楔块型号
|
0.625 x 0.625 |
2.25 |
A430S-SB |
C430-SB |
ABWS-8 -X° |
ABWS-6-X° |
0.625 x 0.75 |
2.25 |
A431S-SB |
C431-SB |
ABWS-8 -X° |
ABWS-6-X° |
0.75 x 0.75 |
2.25 |
A432S-SB |
C432-SB |
ABWS-8 -X° |
ABWS-6-X° |
X°楔块在标准的45°折射剪切波的角度,60钢和70°°。
蜗牛楔尺寸(英寸)
|
(A) |
(B) |
(C) |
(D) |
45° |
2.15 |
0.62 |
1.78 |
1.25 |
60° |
1.91 |
0.65 |
1.81 |
1.25 |
70° |
2.17 |
0.67 |
1.92 |
1.25 |
螺钉之间的距离(中心)1”。
accupath楔尺寸*(英寸)
(in inches)
(A) |
(B) |
(C) |
(D) |
|
45° |
1.50 |
0.90 |
1.96 |
1.50 |
60° |
1.68 |
0.79 |
2.05 |
1.50 |
70° |
1.66 |
0.96 |
2.20 |
1.50 |
螺钉之间的距离(中心)1.062”。
CDS楔块
CDS楔块
CDS楔块可在钢材料中产生30度横波和70度纵波,从而通过30-70-70技术对与内壁相连的裂缝进行定量。
了解CDS
The 30-70-70 crack detection technique uses a single element transducer with a CDS wedge for detection and sizing of ID connected cracks. This technique uses a combination of three waves for sizing flaws of different depths.
该30-70-70裂纹检测技术使用一个单一的元素的传感器与CD楔检测和ID连接裂纹尺寸。这种技术结合使用的胶不同深度的缺陷三波。
•An OD creeping wave creates a 31.5 degree indirect shear, (red in diagram to the left), wave which mode converts to an ID creeping wave; this will produce a reflected signal on all ID connected cracks.
•OD爬波产生一个31.5度的间接剪切,(红色在图左),波的模式转换为一个ID爬波;这将对所有连接的裂缝产生的反射信号。
•A 30 degree shear wave, (yellow in diagram to the left), will reflect off the material ID at the critical angle and mode convert to a 70 degree longitudinal wave; a signal will be received by the transducer on mid-wall deep cracks.
•30度的剪切波,(黄图左边),反映了材料的ID在临界角和模式转换到一个70度的纵向波;信号将通过对中墙深裂缝传感器接收。
•A 70 degree longitudinal wave, (blue in diagram to the left), will reflect off the tip of a deep wall crack.
•70度的纵向波,(蓝图左),反映了一个深刻的墙体裂缝**。
Based on the presence or absence of these three waves, both detection and sizing of ID connected cracks is possible.
基于这三个波的存在或不存在,检测和ID连接裂缝上浆是可能的。
CdS楔块
CDS Wedges are used in the "30-70-70" technique for crack detection and sizing. They are compatible with our replaceable miniature screw-in angle beam transducers, making them an economical alternative to other commercially available products
CdS楔块中使用的“30-70-70”技术对裂纹的检测和上浆。他们与我们的可更换的微型螺旋角光束传感器兼容,使他们对其他市售产品的一种经济的选择
英寸 |
毫米 |
型号 |
0.25 |
6 |
CDS-4T |
0.375 |
10 |
CDS-7T |
ABWS-8 -45°|ABWS-8 60°|ABWS-8 -70° AWS楔块与探头Olympus奥林巴斯 厂家生产代理
ABWS-8 -45°|ABWS-8 60°|ABWS-8 -70° AWS楔块与探头Olympus奥林巴斯 厂家生产代理
ABWS-8 -45°|ABWS-8 60°|ABWS-8 -70° AWS楔块与探头Olympus奥林巴斯 厂家生产代理
ABWS-8 -45°|ABWS-8 60°|ABWS-8 -70° AWS楔块与探头Olympus奥林巴斯 厂家生产代理
ABWS-8 -45°|ABWS-8 60°|ABWS-8 -70° AWS楔块与探头Olympus奥林巴斯 厂家生产代理